The friction stir welding joint of 7N01 aluminum alloy has strong stress corrosion sensitivity due to the inhomogeneity of microstructure. In this paper, the stress corrosion behavior of 14 mm thick plate 7N01-T4 welding joint and base metal was investigated by means of electrochemical impedance spectroscopy, slow strain rate tensile test and electron back scattered diffraction. The results show that the charge transfer resistance of the welding joint is obviously lower than that of the base metal. The lowest impedance at the joint is 698 Ωcm2, but the lowest impedance is 1082 Ωcm2 at the base metal.The lowest Rct value at the weld is only 64.5% of the base metal. The thermal-mechanical affected zone on the rear side is the worst area of the resistance to stress corrosion. There are more deformed grains and larger Schmidt factor close to 0.5 in this area, and the different grain orientation can easily lead to the concentration of internal tensile stress and the formation of crack propagation.

本文言語英語
ページ(範囲)1130-1144
ページ数15
ジャーナルJournal of Materials Research and Technology
15
DOI
出版ステータス出版済み - 2021/11/01

ASJC Scopus 主題領域

  • セラミックおよび複合材料
  • 生体材料
  • 表面、皮膜および薄膜
  • 金属および合金

フィンガープリント

「Stress corrosion behavior of friction stir welding joint of 7N01 aluminum alloy」の研究トピックを掘り下げます。これらがまとまってユニークなフィンガープリントを構成します。

引用スタイル