抄録
The development of aromatic cluster size in heat-treated coals by heating above 500 °C is discussed. Heat treatment of coal was performed at 500, 600, and 700 °C to obtain semicoke samples. The temperature range was above the resolidification temperature of the coal samples. For comparison, a strongly coking coal, Australian Goonyella coal, and a slightly coking coal, Chinese Enshu coal, were used as the sample coals. Analysis of the virgin coals and the semicoke samples with solid-state 13C NMR indicated that the strongly coking coal tended to develop the aromatic ring size to a greater degree than the slightly coking coal as the heat-treatment temperature increased. To examine this tendency, a ruthenium ion catalyzed oxidation reaction was applied to the semicoke samples to obtain information concerning the distribution of the aromatic ring size. The products from this reaction also implied that the semicoke samples obtained from the strongly coking coal had an aromatic ring of larger size on average. A schematic representation of the behavior of molecules in the two coal samples during heating was established.
本文言語 | 英語 |
---|---|
ページ(範囲) | 1709-1715 |
ページ数 | 7 |
ジャーナル | Energy and Fuels |
巻 | 18 |
号 | 6 |
DOI | |
出版ステータス | 出版済み - 2004/11 |
ASJC Scopus 主題領域
- 化学工学一般
- 燃料技術
- エネルギー工学および電力技術