抄録
Significant grain refinement was achieved in a cast Mg-8 mass% Li alloy through processing by equal-channel angular pressing (ECAP) using a die having an internal channel angle of 110° and a pressing temperature of 473 K. Following extrusion and subsequent ECAP through two passes, the alloy exhibited excellent superplastic properties including a maximum elongation of ∼970% at 473 K when using an initial strain rate of 1.0 × 10-4 s-1. The strain rate sensitivities under the optimum superplastic conditions were measured as m ≈ 0.4-0.6. The maximum elongation achieved in this investigation is very high by comparison with other Mg alloys tested in tension at similar temperatures and strain rates.
本文言語 | 英語 |
---|---|
ページ(範囲) | 439-442 |
ページ数 | 4 |
ジャーナル | Materials Science and Engineering A |
巻 | 410-411 |
DOI | |
出版ステータス | 出版済み - 2005/11/25 |
ASJC Scopus 主題領域
- 材料科学一般
- 凝縮系物理学
- 材料力学
- 機械工学