抄録
Effect of precipitate state of Mg2Si as well as Si content in Al-Mg2Si alloys on the reduction of a die-line defect on the surface of extruded products was investigated in industrial scale. The solid product was extruded by 1500 us ton direct extrusion press at billet temprature 460°C, ram speed 9-13 mm/s and extrusion ratio 66.5. When Si content is low and a large amount of coarsened Mg2Si is present in the alloy after homogenization at 400°C for 2 h, the extruded samples have bright smooth surface and nonbright rough surface. When a microscopic Mg2Si is present in the alloy after homogenization at 200°C for 2 h, the extruded samples have high-quality surface with only nonbright and uniform surface roughness. When Si content is high and a large amount of coarsened Mg2Si is present in the alloy after homogenization at 400°C for 2 h, the extruded samples have poor-quality surface with a tearing defect. However, when a microscopic Mg2Si is present in the alloy, which is caused by a widely used homogenizing method or after homogenization at 200°C for 2 h, the samples extruded at ram speed 9-13 mm/s have high-quality surface with only nonbright and uniform surface roughness.
本文言語 | 英語 |
---|---|
ページ(範囲) | 450-455 |
ページ数 | 6 |
ジャーナル | Keikinzoku/Journal of Japan Institute of Light Metals |
巻 | 46 |
号 | 9 |
DOI | |
出版ステータス | 出版済み - 1996/09 |
ASJC Scopus 主題領域
- 材料力学
- 機械工学
- 金属および合金
- 材料化学