The behavior of two step aging in an Al-1.0 mass%Mg2Si-0.4 mass%Si alloy was investigated by high resolution transmission electron microscopy (HRTEM) together with hardness, electrical resistivity measurements. A number of primary G.P. zones with the diameter of about 1nm were observed in the specimen aged at 293 K for 60 ks. Both the mono- and multi-layer G.P. zones were detected in the specimen aged at 343 K for 60 ks. On the contrary, almost no G.P. zones were formed in the specimen aged at 423 K for 60 ks. Instead, a number of random type precipitates were observed. The aging at 473 K produced precipitates in the following sequences: the random type→parallelogram type→β″ phase→TYPE-B→TYPE-A (→partially TYPE-C). The maximum hardness (HVmax) of the specimen aged at 473 K after pre-aging at 293 K for 60 ks indicates a negative effect, i.e. the HVmax of the two step aged specimen is lower than that of the specimen only aged at 473 K. The HVmax of the specimen aged at 473 K after pre-aging at higher temperatures than 343 K shows a positive effect, i.e. the HVmax of the two step aged specimen is higher than that of the specimen only aged at 473 K. In the specimen pre-aged at 423 K which exhibits a positive effect, a number of the random type precipitates are formed. On the other hand, in the specimen pre-aged at 293 K, which exhibits a negative effect, a number of the β″ phase are formed. It is concluded that the random type precipitates produced at 423 K pre-aging are stable at the 473 K final aging, while the primary G.P. zones produced after pre-aging at 293 K become unstable at the 473 K final aging due to dissolution into the matrix, resulting in the heterogeneous precipitation of the β″ phase.

Original languageEnglish
Pages (from-to)827-833
Number of pages7
JournalNippon Kinzoku Gakkaishi/Journal of the Japan Institute of Metals
Volume62
Issue number9
DOIs
StatePublished - 1998/09

Keywords

  • Aluminum-magnesium-silicon alloy
  • Guinier-Preston zone
  • High resolution transmission electron microscopy
  • Precipitation
  • Two step aging

ASJC Scopus subject areas

  • Condensed Matter Physics
  • Mechanics of Materials
  • Metals and Alloys
  • Materials Chemistry

Fingerprint

Dive into the research topics of 'Precipitation behavior of a two-step aged Al-Mg-Si alloy with excess silicon'. Together they form a unique fingerprint.

Cite this